Structural Materials |
Research progress of high strength and
heat resistant Mg-Gd-Y-Zr alloys |
WU Wen-xiang, JIN Li, DONG Jie, ZHANG Zhen-yan, DING Wen-jiang |
2709 |
Research progress on effect of precipitation on
deformation mechanism of magnesium alloys |
SONG Bo, XIN Ren-long, LIU Qing |
2719 |
Dynamic mechanical behavior and deformation mechanism of
extruded AM30 magnesium alloy |
WANG Chang-yi, LIU Zheng, MAO Ping-li |
2732 |
Effect of hot rolling on microstructure and mechanical properties of welded joints of AZ31 magnesium alloy |
CHU Ya-jie, LI Xiao-quan, WU Shen-qing |
2739 |
Rapid growth of primary α-Fe phase from undercooled Fe-Mo alloys |
ZHANG Bo, LU Xiao-yu, DAI Fu-ping, RUAN Ying |
2744 |
Deformation rule and mechanism in compress process of
aluminium alloy square ring |
LI Feng, XU Yong-chao, LI Chao, LIU Xiao-jing |
2751 |
Exfoliation corrosion and electrochemical impedance spectroscopy of Al-Cu-Li alloy containing Sc |
LIANG Wen-jie, PAN Qing-lin, HE Yun-bin |
2757 |
Effect of withdrawal rate on microstructure of
directionally solidified Ni-45Ti-5Al alloys |
YANG Chun-lei, ZHENG Li-jing, LI Yan, ZHOU Lei, ZHANG Hu |
2763 |
Effect of Er on microstructure and properties of Ti-16Al-27Nb alloy |
SUN Yan-ran, DUAN Hui-ping, KANG Ning |
2769 |
Static recrystallization behavior of Zn-1.0Cu-0.2Ti alloy |
XIAO Lai-rong, ZHANG Xi-min, WANG-Yan, ZENG De-lu, ZHANG Hong-ling, LI Wei |
2775 |
Influence of vacuum stress relieving annealing on residual stress and microstructure properties of TC18 titanium alloy |
ZHANG Yao-wu, ZENG Wei-dong, SHI Chun-ling, KANG Chao, PENG Wen-wen |
2780 |
Effect of aging treatment on microstructure and
mechanical properties of deformation-processed
Cu-10Fe-3Ag in-situ composite |
LI Yong, YI Dan-qing, LIU Rui-qing, SUN Shun-ping |
2786 |
Functional Materials |
Fabrication and corrosion properties of
MgO/Mg biocomposite materials |
TANG Wei, LEI Ting, LI Nian-feng |
2792 |
Ignition-proof mechanics of surface film of Mg-Y-Ce alloy system |
FAN Jian-feng |
2799 |
Effect of Si4+ and F− doping on structure and
electrochemical properties of LiNi1/3Co1/3Mn1/3O2 |
ZHANG Pei-xin, ZHANG Li, TAN Zhi-bo, REN Xiang-zhong |
2805 |
Capacity fading mechanism of LiMn2O4 cell after storage |
LIU Yun-jian, SONG Yang, WEI Hong-bing, WANG Cai-juan, ZHAO Yong, JIN Ting, LI Xin-hai, GUO Hua-jun
| 2812 |
Hydrogen evolution reaction activity of
electrodeposited amorphous/nanocrystalline Ni-Mo-La alloy electrode |
GAO Cheng-hui, LI Ning |
2819 |
Effect of filament radiation length and W-C gradient interlayer on diamond films deposited on high-speed steel |
WEI Qiu-ping, YU Zhi-min, CHEN Zhong, ZHU Xiao-dong, LIU Pei-zhi |
2825 |
Effect of SiC coating on ablation resistance of
C/C composites under oxyacetylene torch flame |
SU Zhe-an, YANG Xin, HUANG Qi-zhong, HUANG Bai-Yun, LI Jian-li, ZHANG Ming-yu, XIE Zhi-yong |
2838 |
Fe-Ni-B-Si-Nb amorphous and nanocrystalline composite coating
prepared by laser cladding and remelting |
ZHANG Pei-lei, YAN Hua, XU Pei-quan, YU Zhi-shui, LI Zhu-guo, YAO Cheng-wu |
2846 |
High temperature erosion resistance of
FeMnCrAl/Cr3C2 coatings deposited by high velocity arc spraying |
LUO Lai-ma, LIU Shao-guang, YAO Ji-peng, LI Jian, WU Yu-cheng |
2852 |
Preparation and properties of (110) preferred orientation
La2/3Sr1/3MnO3 film deposited on Si (100) substrate |
LI Ting-xian, ZHANG Ming, WANG Guang-ming, GUO Hong-rui, LI Kuo-she, LI Xi-lu, ZHOU Wen-long, YAN Hui< |
2857 |
Fabrication and properties of TiN/β′-Sialon electroconductive
composites from high titania slag-based mixture |
JIANG Tao, XUE Xiang-xin, LI Jiang, DUAN Pei-ning |
2863 |
Structure, phase transformation and magnetic properties in
polycrystalline Ni47Mn32Ga21 directionally solidified alloy |
CAI Pei-yang, FENG Shang-shen, XUE Shuang-xi, CHEN Wei-ping, ZHOU Ying, WU Jian-bo, WANG Gu-ping |
2869 |
Influence of composite surfactant on print gloss of bronze powder |
BAI Yan-xia, HUI Tao, ZHAO Mai-qun, JIN Li |
2875 |
Computational Materials Scien |
High temperature flow stress behavior of
as-extruded 7075 aluminum alloy and neural network constitutive model |
WANG Yu, SUN Zhi-chao, LI Zhi-ying, YANG He |
2880 |
Interface debonding properties of
carbon nanotube-reinforced magnesium matrix composites |
ZHU Jie, LI Wei-xue, DAI Jian-feng, WANG Qing |
2888 |
3D simulation of electromagnetic tube bulging based on
loose coupling method |
CUI Xiao-hui, MO Jian-hua, HE Wen-zhi |
2896 |
Controllable growth of crystal morphology of Ni jet-electrodeposition |
TIAN Zong-jun, WANG Gui-feng, LIU Zhi-dong, SHEN Li-da, HUANG Yin-hui |
2903 |
Inhomogeneity of micro-arc oxidation of V-shaped aluminum cavity |
MA Ying-he, GONG Chun-zhi, TIAN Xiu-bo, YANG Shi-qin |
2909 |
Numerical simulation of
smelting process in copper flash smelters at high loading rate |
CHEN Zhuo, WANG Yun-xiao, SONG Xiu-ming, ZHAO Rong-sheng, YIN Shu-gui |
2916 |
Soft sensor modeling for slag composition of
silicon-manganese smelting process |
TANG Chun-xia, JIANG Tong, YANG Chun-hua, HE Jian-jun |
2922 |
Mine |
Leaching mechanism of willemite in (NH4)2SO4-NH3-H2O system |
LIU Zhi-yong, LIU Zhi-hong, CAO Zhi-yan, LI Qi-hou, YANG Tian-zu |
2929 |
Potential—pH diagrams for V-Fe-H2O system during oxygen pressure
acid leaching of vanadium-bearing converter slags |
ZHANG Ting-an, MU Wang-zhong, DOU Zhi-he, LÜ, Guo-zhi, LIU Yan |
2936 |
Sodium hydroxide digestion of wolframite by reactive extrusion |
ZHAO Zhong-wei, LIANG Yong, LIU Xu-heng, LI Hong-gui, CHEN Ai-liang, LIANG Xin-xing |
2946 |
Thermodynamic analysis of lead sulfide flash smelting process |
WANG Jin-liang, ZHANG Wen-hai, ZHANG Chuan-fu |
2952 |
Decomposition kinetics of iron ore tailings by
NaOH-NaNO3 molten salt method |
YU Hong-hao, HE Yan, XUE Xiang-xin, WANG Yu-lian |
2958 |
Leaching nickel and removing Fe from
garnierite of transition layer nickel laterite ores |
WANG Duo-dong, ZHAO Zhong-wei, CHEN Ai-liang, HUO Guang-sheng, CHEN Xing-yu |
2964 |
Adsorption properties of nano-TiO2 for Cd(Ⅱ) |
LIU Xue-yan, YANG Li-jun, JIN Yan-li, ZHANG Lei, XU Tian-ci, LI Na |
2971 |