(宝钛集团有限公司,宝鸡 721014)
摘 要: 研究3 mm厚的钛/钢复合板在爆炸焊接工艺技术条件下,采用不同药量的低爆速炸药,通过从起爆端开始沿爆轰长度方向对结合界面进行波纹检测及氧化和熔化研究,研究低爆速炸药不同用药量时在钛/钢复合板的稳定爆轰长度,为长度≥4 m钛/钢复合板爆炸焊接工艺参数的制定建立基础。
关键字: 钛/钢复合板;低爆速炸药;爆轰载荷;稳定长度
(Baoti Group Co., Ltd., Baoji 721014, China)
Abstract:By utilizing low detonation velocity explosive technology, the explosive welding of the 3 mm-thickness layer of titanium/steel clad plate was studied. The oxidation and melting of the interface from the detonation spreading direction was studied. Accordingly, a base for the parameters for the explosive welding of titanium/steel clad plate with length over 4 m was set up.
Key words: titanium/steel clad plate; low detonation velocity explosives; detonation load; stability length