(北京理工大学 机电工程学院, 北京 100081)
摘 要: 通过实验分析了90W和93W钨合金在动加载时其断裂机理及特性以及侵彻时其微观结构响应的异同点。通过对比发现,二者的断裂机理基本相似,但侵彻时,由于90W钨合金中存在较多的粘结相而使得其蘑菇头较小,其中的钨颗粒变形也较小;只在93W钨合金中发现了绝热剪切现象的征候
关键字: 钨合金; 动态断裂; 侵彻; 绝热剪切
alloy under impact dynamics
(College of Electro-mechanical Engineering,
Beijing Insitute of Technolog,Beijing 100081, P.R.China)
Abstract:The difference of micro-behavior between 90W and 93W tungsten alloy under impact dynamics was analysed. Their fracture feature is alike. But when penetrating, because of more matrixes in 90W, the end of penetrator of 90W is smaller and its shape changing of W grains is also smaller. So, only in 93W, the adiabatic shearing bands can be found.
Key words: tungsten-alloy; dynamic fracture; penetration; adiabatic shearing