Transactions of Nonferrous Metals Society of China The Chinese Journal of Nonferrous Metals

您目前所在的位置:首页 - 期刊简介 - 详细页面

中国有色金属学报(英文版)

Transactions of Nonferrous Metals Society of China

Vol. 30    No. 8    August 2020

[PDF Download]        

    

Effect of Sn on synthesis of nanocrystalline Ti-based alloy with fcc structure
C. AGUILAR1, E. PIO1, A. MEDINA2, C. PARRA1, R. MANGALARAJA3, P. MARTIN1, I. ALFONSO4, K. TELLO1

1. Departamento de Ingeniería Metalúrgica y de Materiales, Departamento de Física (+) Universidad Técnica Federico Santa María, Valparaíso, Chile;
2. Instituto de Investigación en Metalurgia y Materiales, Universidad Michoacana de San Nicolás de Hidalgo, Morelia, México;
3. Laboratorio de Cerámicos Avanzados y Nanotecnologia, Departamento de Ingeniería de Materiales, Universidad de Concepción, Concepción, Chile;
4. Instituto de Investigaciones en Materiales, Universidad Nacional Autónoma de México, Campus Morelia UNAM, Morelia, México

Abstract:The effect of the amount of Sn on the formation of fcc phase in Ti-13Ta-xSn (x=3, 6, 9 and 12, at.%) alloys was studied. The alloys were synthesized by mechanical alloying using a planetary mill, jar and balls of stabilized yttrium. Using Rietveld refinement, it was found that the obtained fcc phase has crystallite size smaller than 10 nm and microstrain larger than 10-3. Both conditions are required to form an fcc phase in Ti-based alloys. For all samples, the microstructure of the fcc phase consists of equiaxial crystallites with sizes smaller than 10 nm. The largest presence of fcc phase in the studied Ti alloy was found with 6 at.% Sn, because this alloy exhibits the largest microstrain (1.5×10-2) and crystallite size of 6.5 nm. Experimental data reveal that a solid solution and an amorphous phase were formed during milling. The necessary conditions to promote the formation of solid solution and amorphous phases were determined using thermodynamic calculations. When the amount of Sn increases, the energy required to form an amorphous phase varies from approximately 10 to approximately -5 kJ/mol for 3 and 12 at.% Sn, respectively. The thermodynamic calculations are in agreement with XRD patterns analysis and HRTEM results.

 

Key words: Ti-based alloy; phase transformation; fcc phase; Rietveld analysis; mechanical alloying

ISSN 1004-0609
CN 43-1238/TG
CODEN: ZYJXFK

ISSN 1003-6326
CN 43-1239/TG
CODEN: TNMCEW

主管:中国科学技术协会 主办:中国有色金属学会 承办:中南大学
湘ICP备09001153号 版权所有:《中国有色金属学报》编辑部
------------------------------------------------------------------------------------------
地 址:湖南省长沙市岳麓山中南大学内 邮编:410083
电 话:0731-88876765,88877197,88830410   传真:0731-88877197   电子邮箱:f_ysxb@163.com