中国有色金属学报(英文版)
Transactions of Nonferrous Metals Society of China
Vol. 3 No. 4 December 1993 |
(Department of Chemistry; Central South Unirersity of Technology; Changsha 410083; China)
Abstract:After Cu-Ni ore powder pre-soaked in AlCl3 solution.the leaching ratios of copper and nickel can increase obviously.By X-ray diffraction analyses,electron energy spectrum analyses and electrochemical experiments,it is affirmed that,the activation of aluminum ion includes two aspects:one is the surface change of the ore by the absorption of hydrolysates,and the oth- er is the change of semiconductor characteristics of the metal sulfides by impurity aluminum ion entering the lattice,so that leaching reactions are accelerated.
Key words: oxidative leaching; copper-nickel sulfide ore; aluminium chloride; activation