Macro- and microstructural changes
in-hydrogenated TiMn2 and Ta
S. Semboshi,  N. Masahashi, S. Hanada

Institute for Materials Research, Tohoku University, Sendai 980-8577, Japan

Abstract:Binary TiMn2 alloys with various compositions were arc melted in an Ar atmosphere. These alloys consist of TiMn2 and a small amount of TiMn depending on alloy composition. Annealed Ti-59.4%Mn exhibits the greatest capacity for hydrogen absorption and the smallest degradation of capacity during repeated hydrogen absorption and desorption. No apparent macro- and microstructural changes are observed in Ti-59.4%Mn by repeated hydrogenation of 30 cycles. At Mn content higher than 59.4%Mn, the formation of nano-sized Ti-hydride and the lattice expansion due to retained interstitial hydrogen were confirmed in repeatedly hydrogenated alloys. Pulverized powders were refined in all the alloys with in creasing the number of repeated hydrogenation cycles. Many onion-like cracks are introduced in annealed pure Ta with 100μm equi-axed grains by holding at 1473K followed by furnace cooling to room temperature in a hydrogen atmosphere, but no crack is observed after holding at 1473K in a hydrogen atmosphere followed by furnace cooling in an Ar atmosphere. It is concluded that the surface activation is attained in a hydrogen atmosphere at 1473K and multiple cracking occurs by absorbing a large amount of hydrogen at lower temperature. Volume expansion and dislocations generated b y hydrogenation and hydride formation are responsible for multiple cracking. Hydrogen-induced multiple cracking in Ta occurs in the following sequence: hydrogen absorption, lattice expansion, hydride formation, and crack nucleation and propagation. Powder fabrication of Ta by hydrogenation is discussed in comparison with the hydrogen pulverization of intermetallic alloys.

 

Key words: macrostructure; microstructure; hydrogen absorbing alloy

ISSN 1004-0609
CN 43-1238/TG
CODEN: ZYJXFK

ISSN 1003-6326
CN 43-1239/TG
CODEN: TNMCEW

主管:中国科学技术协会 主办:中国有色金属学会 承办:中南大学
湘ICP备09001153号 版权所有:《中国有色金属学报》编辑部
------------------------------------------------------------------------------------------
地 址:湖南省长沙市岳麓山中南大学内 邮编:410083
电 话:0731-88876765,88877197,88830410   传真:0731-88877197   电子邮箱:f_ysxb@163.com