Structural Materials |
Effects of solution and aging on microstructure and properties of
Al-Zn-Mg-Sc-Zr alloy sheet |
SHANG Bao-chuan, YIN Zhi-min, ZHOU Xiang, HE Zhen-bo, LIN Sen |
2063 |
Effects of multiple precipitates on electrical conductivity of
aged Al-Mg-Si alloys |
YUAN Sheng-ping, PU Xiong, ZHANG Guo-jun, LIU Gang, WANG Rui-hong, SUN Jun, CHEN Kang-hua |
2070 |
Hot-compressive deformation behavior of
semi-continuous cast AZ31B magnesium alloy |
YU Kun, CAI Zhi-yong, XUE Xin-ying, CHEN Fu-wen, TAN Xin, HU Ya-nan |
2075 |
Effects of phosphorus modification on morphology of
primary silicon particles and mechanical properties of
wrought Al-17.5Si-4.5Cu-1Zn-0.7Mg-0.5Ni alloy |
HE Ke-zhun, YU Fu-xiao, ZHAO Da-zhi, ZUO Liang |
2081 |
Effect of prestretching on fracture toughness of
7050 aluminum alloy |
HAN Nian-mei, ZHANG Xin-ming, LIU Sheng-dan, SONG Feng-xuan |
2088 |
Flow stress behavior of 2E12 aluminum alloy during
hot plastic deformation at high temperature |
HUANG Yu-jin, CHEN Zhi-guo, SHU Jun, LIU Yao-qiong, ZHOU Xian |
2094 |
Homogenization treatment and microstructure of
semicontinous casting ingot of 2D70 heat-resistance aluminum alloy |
LI Pei-yue, XIONG Bai-qing, ZHANG Yong-an, LI Zhi-hui,WANG Guo-jun, WANG Feng, ZHU Bao-hong |
2101 |
Microstructure and properties of creep aged 2124 aluminum alloy |
DENG Yun-lai, ZHOU Liang, JIN Kun, ZHANG Xin-ming |
2106 |
Effect of mass fraction of mischmetal addition on
microstructures of A356 alloy |
TANG Xiao-long, PENG Ji-hua, HUANG Fang-liang, XU De-ying, DU Ri-sheng |
2112 |
Hardenability of 2124 aluminum alloy based on
Jominy end quench test |
LIU Jun-cheng, ZHANG Yong-an, LIU Hong-wei, LI Xi-wu, LI Zhi-hui, ZHU Bao-hong, XIONG Bai-qing |
2118 |
Influence of strain rate on stress induced martensitic transformation in
β solution treated Ti-10V-2Fe-3Al alloy |
CHEN Wei , SUN Qiao-yan , XIAO Lin , SHE Wen-bo , SUN Jun , GE Peng |
2124 |
Corrosion mechanism of γ-TiAl alloy at high temperature in
molten salt environment |
XU Bo-wen, ZHAO Wen-yue, MA Yue, GONG Sheng-kai |
2130 |
Effects of heat treatment on microstructure and properties of Ti60 Alloy |
JIA Wei-ju, ZENG Wei-dong, ZHANG Yao-wu, ZHOU Yi-gang |
2136 |
Relationship between precipitate and creep property of
Ti600 high-temperature alloy |
XIN She-wei,HONG Quan, LU Ya-feng, XI Zheng-ping, GUO Ping, QI Yun-lian, ZENG Li-ying |
2142 |
Texture and its influence on tensile and recoverable properties of
hot-rolled Ni47Ti44Nb9 shape memory alloy sheet |
YAN Ying, JIN Wei, ZHOU Ting-jun |
2148 |
Precipitation behavior of TCP phase and its influence on stress rupture property of single crystal nickel-based superalloys |
TIAN Su-gui, QIAN Ben-jiang, LI Tang, YU Li-li, WANG Ming-gang |
2154 |
Effect of pore-forming agent on microstructure and thermal conductivity of SiCp/Al composites prepared by pressureless infiltration |
WANG Qing-ping, WU Yu-cheng, PAN Rong-jun, HONG Yu, MIN Fan-fei |
2162 |
Effect of alloying elements on oxidation behavior of
Co-Al-W alloys at high temperature |
XU Yang-tao, XIA Tian-dong, YAN Jian-qiang, ZHAO Wen-jun |
2168 |
Functional Materials |
Effect of inoculant parameters on AM60 Mg alloy
semisolid slurry prepared by self-inoculation method (Ⅱ) |
LI Yuan-dong, YANG Jian, MA Ying, QU Jun-feng, ZHANG Peng |
2178 |
Phase transition strain and magnetic-field-induced strain in Ni46Cu4Mn38Sn12 Heusler alloy |
LI Zhe, JING Chao, QIAO Yan-fei , ZHANG Hao-lei, CAO Shi-xun, ZHANG Jin-cang, SUN Liang |
2187 |
Effect of CeO2 on microstructure and wear resistance of
Cr-Al coating by slurry packing on copper |
WANG Hong-xing, LI Ying-guang |
2192 |
Influence of final-annealing and pretreatment before etching on
pitting ability of aluminum foils |
LIU Jian-cai, ZHANG Xin-ming, CHEN Ming-an, ZHU Bin, TANG Jian-guo, LIU Sheng-dan |
2199 |
Preparation and electrochemical properties of
branched LiFePO4/C composite with carbon core structure |
CHEN Han, GONG Wen-qiang, LIU You-liang, LIU Jian-hua |
2206 |
Raman spectrum and inhibition effect of self-assembled monolayers of ammonium pyrrolidine dithiocarbamate on copper surface |
YUE Zhong-wen, LIAO Qiang-qiang, WANG Zuo-hua, LI Yi-jiu, CHEN Ya-qiong, GE Hong-hua |
2213 |
In-situ growth of silver nanoparticle on glass substrates and
its surface-enhanced Raman scattering |
YI Zao, LI Kai, HAN Shang-jun, NIU Gao, YI You-gen, CHEN Shan-jun, LUO Jiang-shan, TANG Yong-jian,
| 2221 |
Mine |
Effect of Tween80 on flotation of diaspore |
FENG Qi-ming, ZHANG Jing, LU Yi-ping , OU Le-ming, ZHANG Guo-fan |
2228 |
Pretreatment for V-bearing steelmaking slag by
beneficiation methods and its effect on followed leaching procedure |
YE Guo-hua, TONG Xiong, LU Lu |
2233 |
Depression effect of azo organic depressants on sulphide minerals |
CHEN Jian-hua, LIANG Mei-lian, LAN Li-hong |
2239 |
Theory study on chemical reactivity of 2-mercaptobenzothiazole, 2-mercaptobenzoxazole and 2-mercaptobenzimidazole in solution |
LIU Guang-yi, ZHAN Jin-hua, ZHONG Hong, XIA Liu-yin, WANG Shuai |
2248 |
Synthesis and extraction performance of di-decylphosphinic acid |
JU Zhong-jun, LI Lin-yan, XU Sheng-ming, WANG Cheng-yan, LIAO Fu-hui, LI Guo-bao |
2254 |
φ—pH diagram of Li-Ti-H2O system at 298.15 K and
synthesis of Li4Ti5O12 |
QIU Wen-shun, LI Yun-jiao, ZHAO Zhong-wei, HUO Guang-sheng, XI Xiao-ming, CHEN Pan-pan |
2260 |