Structure and electrochemical properties of Li(Ni0.5Mn0.5)1−xTixO2 prepared by one-step solid state reactio |
CAO Si-hai(曹四海), WANG Zhi-xing(王志兴), LI Xin-hai(李新海),GUO Hua-jun(郭华军), PENG Wen-jie(彭文杰), YIN Zhou-lan(尹周澜) |
1247 |
Characteristics and properties of surface coated nano-TiO2 |
GAO Jia-cheng(高家诚), ZOU Jian(邹健),TAN Xiao-wei(谭小伟), WANG Yong(王勇) |
1252 |
Microdefects and electron densities in NiTi shape memory alloys studied by positron annihilation |
HU Yi-feng(胡益丰), DENG Wen(邓文), HAO Wen-bo(郝文博),YUE Li(岳丽), HUANG Le(黄乐), HUANG Yu-yang(黄宇阳), XION |
1259 |
Measurement and analyses of molten Ni-Co alloy density |
XIAO Feng(肖锋), K. MUKAI, FANG Liang(方亮),FU Ya(傅亚), YANG Ren-hui(杨仁辉) |
1263 |
Simulation on function mechanism of T1(Al2CuLi) precipitate in localized corrosion of Al-Cu-Li alloys |
LI Jin-feng(李劲风), ZHENG Zi-qiao(郑子樵), REN Wen-da(任文达) ,CHEN Wen-jing(陈文敬), ZHAO Xu-shan(赵旭山), LI Shi-chen(李世晨) |
1268 |
Dynamic explicit FE modeling of hot ring rolling process |
WANG Min(王敏), YANG He(杨合), SUN Zhi-chao(孙志超),GUO Liang-gang(郭良刚), OU Xin-zhe(欧新哲) |
1274 |
Reactions between Ti and Ti3SiC2 in temperature range of 1 273−1 573 K |
GU Wan-li(谷万里), ZHOU Yan-chun(周延春) |
1281 |
Properties of electrodeposited amorphous Fe-Ni-W alloy deposits |
HE Feng-jiao(何凤姣), WANG Miao(王淼), LU Xin(陆欣) |
1289 |
Effects of H2O2 pretreatment on surface characteristics and bioactivity of NaOH-treated NiTi shape memory alloy |
CHU Cheng-lin(储成林), HU Tao(胡涛), ZHOU Jun(周俊),PU Yue-pu(浦跃朴), YIN Li-Hong(尹立红), DONG Yin-sheng(董寅生),& |
1295 |
Influence of process parameters on electrochemical and physical properties of sputtered iron-doped nickel oxide thin films |
HUANG Jin-zhao(黄金昭), XU Zheng(徐征), LI Hai-ling(李海玲),KANG Guo-hu(亢国虎), WANG Wen-jing(王文静) |
1301 |
Recrystallization behavior of high purity aluminum at 300 ℃ |
DU Yu-xuan(杜予晅), ZHANG Xin-ming(张新明),YE Ling-ying(叶凌英), LUO Zhi-hui(罗智辉) |
1307 |
Microstructure evolution of processed Mg-Al-Zn alloy by equal channel angular extrusion in semi-solid isothermal treatment |
JIANG Ju-fu(姜巨福), LUO Shou-jing(罗守靖) |
1313 |
Inner-product of strain rate vector through direction cosine in coordinates for disk forging |
ZHAO De-wen(赵德文), JIN Wen-zhong(金文忠),WANG Lei(王磊), LIU Xiang-hua(刘相华) |
1320 |
Stability of electrodeposited amorphous Ni-Fe-P alloys |
GAO Cheng-hui(高诚辉) |
1325 |
Thermal expansion anomaly and spontaneous magnetostriction of Dy2AlFe14Mn2 compound |
WANG Hai-yun(王海云), ZHAO Miao(赵淼), GAO Yan(高艳),ZHOU Yan(周严), FU Bin(傅斌), YAN Da-li(严达利) |
1331 |
Tensile property of Al-Si closed-cell aluminum foam |
YU Hai-jun(尉海军), YAO Guang-chun(姚广春), LIU Yi-han(刘宜汉) |
1335 |
Effect of large cold deformation after solution treatment on precipitation characteristic and deformation strengthening of 2024 and 7A04 aluminum alloys |
NING Ai-lin(宁爱林), LIU Zhi-yi(刘志义), ZENG Su-min(曾苏民) |
1341 |
Preparation of silver nanoparticle via active template under ultrasonic |
ZHENG Min(郑敏), WANG Zuo-shan(王作山), ZHU Ya-wei(朱亚伟) |
1348 |
Numerical simulation in powder compaction of metallurgy component |
HUANG Chun-man(黄春曼), CHEN Pu-qing(陈普庆),SHAO Ming(邵明), LI Yuan-yuan(李元元) |
1353 |
Preparation of ITO transparent conductive film by sol-gel method |
LI Zhi-hua(李芝华), REN Dong-yan(任冬燕) |
1358 |
Effects of constitutive parameters on adiabatic shear localization for ductile metal based on JOHNSON-COOK and gradient plasticity models |
WANG Xue-bin(王学滨) |
1362 |
Magnetic properties of nanostructural γ-Ni-28Fe alloy |
LIU Yin(刘银), QIN Xiao-ying(秦晓英), QIU Tai(丘泰) |
1370 |
Effect of diode-laser parameters on shear force of micro-joints soldered with Sn-Ag-Cu lead-free solder on Au/Ni/Cu pad |
WANG Jian-xin(王俭辛), XUE Song-bai(薛松柏), FANG Dian-song(方典松),JU Jin-long(鞠金龙), HAN Zong-jie(韩宗杰), YAO Li-hua(姚立华)< |
1374 |
Optimized constitutive equation of material property based on inverse modeling for aluminum alloy hydroforming simulation |
LANG Li-hui(郎利辉), LI Tao(李涛), ZHOU Xian-bin(周贤宾),B. E. KRISTENSEN, J. DANCKERT, K. B. NIELSEN |
1379 |
Numerical simulation on forging process of TC4 alloy mounting parts |
LÜ, Cheng(吕成), ZHANG Li-wen(张立文) |
1386 |
Growth behavior of interfacial compounds in galvanized steel joints with CuSi3 filler under arc brazing |
YU Zhi-shui(于治水), LI Rui-feng(李瑞峰), QI Kai(祁凯) |
1391 |
Growth and corrosion behavior of rare earth film on hot-dip galvanized steel |
LU Jin-tang(卢锦堂), WU Hai-jiang(吴海江), KONG Gang(孔纲),CHE Chun-shan(车淳山), XU Qiao-yu(许乔瑜) |
1397 |
Influence of process factors on shape memory effect of CuZnAl alloys |
LIU Hai-xia(刘海霞), SI Nai-chao(司乃潮), XU Gui-fang(徐桂芳) |
1402 |
Two-dimensional cellular automaton model for simulating structural evolution of binary alloys during solidification |
ZHANG Lin(张林), ZHANG Cai-bei(张彩碚) |
1410 |
Extraction and purification of magnetic nanoparticles from strain of Leptospirillum ferriphilum |
GAO Jian(高健), XIE Jian-ping(谢建平), DING Jian-nan(丁建南),KANG Jian(康健), CHENG Hai-na(程海娜), QIU Guan-zhou(邱冠周)< |
1417 |
Correlation analysis on partition of rare earth in ion-exchangeable phase from weathered crust ores |
CHI Ru-an(池汝安), DAI Zu-xu(戴祖旭), XU Zhi-gao(徐志高),WU Yuan-xin(吴元欣), WANG Cun-wen(王存文) |
1421 |
Application of cetylpyridinium chloride in dispersion of antibacterial ceramic glaze |
CHAI Li-yuan(柴立元), CHENG Ming-ming(程明明), PENG Bing(彭兵),HUANG Yi(黄毅), ZHANG Xiao-fei(张晓飞) |
1426 |
Biosorption behaviors of Cu2+, Zn2+, Cd2+ and mixture by waste activated sludge |
LUO Sheng-lian(罗胜联), YUAN Lin(袁林), CHAI Li-yuan(柴立元),MIN Xiao-bo(闵小波), WANG Yun-yan(王云燕),FANG Yan(方 |
1431 |
Structure and resistance of concentration polar layer on cation exchange membrane-solution interface |
SANG Shang-bin(桑商斌), HUANG Ke-long(黄可龙),LI Xiao-gang(李晓刚), WANG Xian(王显) |
1436 |
Treatment of naphthalene derivatives with iron-carbon micro-electrolysis |
WANG Yu-ping(王玉萍), WANG Lian-jun(王连军),PENG Pan-ying(彭盘英), LU Tian-hong(陆天虹) |
1442 |
Extraction of indium from indium-zinc concentrates |
LI Shi-qing(李仕庆), TANG Mo-tang(唐谟堂), HE Jing(何静),YANG Sheng-hai(杨声海), TANG Chao-bo(唐朝波),CHEN Yong-ming |
1448 |
Mathematical module for countercurrently fractional chiral extraction and its VB simulation |
TANG Ke-wen(唐课文), HUANG Ke-long(黄可龙),YI Jian-min(易健民), ZHANG Guo-li(张国丽) |
1455 |
Corrosion behavior of pure aluminum in FeCl3 solution |
QU Jun-e(屈钧娥), GUO Xing-peng(郭兴蓬),WANG Hai-ren(王海人), HUANG Jin-ying(黄金营) |
1460 |